Iglasi ye-Erbium kunye ne-ytterbium co-doped phosphate inesicelo esibanzi ngenxa yeempawu ezibalaseleyo.Ubukhulu becala, yeyona nto ibalaseleyo yeglasi ye-1.54μm yelaser ngenxa yobude bayo obukhuselekileyo beliso le-1540 nm kunye nosulelo oluphezulu kwiatmosfera.Ikwafanelekile kwizicelo zonyango apho imfuno yokhuselo lwamehlo inokuba nzima ukulawula okanye ukunciphisa okanye ukuthintela uqwalaselo olubalulekileyo lwembonakalo.Kutshanje isetyenziswe kunxibelelwano lwefiber optical endaweni ye-EDFA yokongeza kwayo.Kukho inkqubela phambili enkulu kulo mmandla.
I-Erbium Glass ifakwe i-Er 3+ kunye ne-Yb 3+ kwaye ifanele izicelo ezibandakanya amazinga aphezulu okuphindaphinda (1 - 6 Hz) kunye nokumpontshwa nge-1535 nm laser diodes.Le glasi ifumaneka ngamanqanaba aphezulu e-Erbium (ukuya kwi-1.7%).
I-Erbium Glass ine-Er 3+, Yb 3+ kunye ne-Cr 3+ kwaye ilungele izicelo ezibandakanya ukumpompa isibane se-xenon.Le glasi isoloko isetyenziswa kwi-laser range finder (LRF) izicelo.
Iinkcazelo ngeempawu ezisisiseko:
Into | Iiyunithi | Er,Yb:Iglasi | Er,Yb,Cr:Glass |
Ubushushu benguqu | ºC | 556 | 455 |
Ubushushu obuthambileyo | ºC | 605 | 493 |
Coeff.yoLwandiso lweThermal oluLula (20~100ºC) | 10‾⁷/ºC | 87 | 103 |
I-Thermal Conductivity (@ 25ºC) | W/m.ºK | 0.7 | 0.7 |
Ukuqina kweMichiza (@100ºC ireyitha ireyithi yelahleko yamanzi adiliweyo) | ug/hr.cm2 | 52 | 103 |
Ukuxinana | g/cm2 | 3.06 | 3.1 |
I-Laser Wavelength Peak | nm | 1535 | 1535 |
Icandelwana elinqamlezileyo loKhuselo oluVunyiweyo | 10‾²º cm² | 0.8 | 0.8 |
UBomi beFluorescent | ms | 7.7-8.0 | 7.7-8.0 |
Refractive Index (nD) @ 589 nm | 1.532 | 1.539 | |
Refractive Index (nD) @ 589 nm | 1.524 | 1.53 | |
dn/dT (20~100ºC) | 10‾⁶/ºC | -1.72 | -5.2 |
Thermal Coeff.yoBubude beNdlela yokubona (20~100ºC) | 10‾⁷/ºC | 29 | 3.6 |
I-Standard Doping
Ukwahluka | Er 3+ | Yb 3+ | Cr 3+ |
Er:Yb:Cr:Glass | 0.13×10^20/cm3 | 12.3×10^20/cm3 | 0.15×10^20/cm3 |
Er:Yb:Iglasi | 1.3×10^20/cm3 | 10×10^20/cm3 |